Fasten rather than weld
7075 is not arc weldable, so assemblies are normally bolted or riveted.
7075 is an aluminium alloy with 5.1 to 6.1% zinc plus magnesium and copper. It is one of the strongest aluminium alloys: in the T6/T651 temper its tensile strength beats mild steel, at about a third of the weight.

Figures from one named manufacturer or industry data sheet, compared with our other CNC metals. See every material side by side in the property comparison.
Data source: Wikipedia: 7075 aluminium alloy (T651; conductivity is the low end of 130–150). Typical values, not guaranteed minimums.
Guide only. General ratings for prototyping, not a recommendation for your application. Filter every material by these needs.
Every material has trade-offs. Knowing them up front saves time and money.
| Aluminium 6061 | Aluminium 7075 | Aluminium 5083 | |
|---|---|---|---|
| Tensile strength MPa | 310 | 570 | 305 |
| Density g/cm³ | 2.7 | 2.81 | 2.66 |
| Stiffness GPa | 68 | 71.7 | 70.3 |
| Thermal conductivity W/m·K | 152 | 130 | 120 |
| Character | General purpose, heat-treatable | High strength | Marine grade, not heat-treatable |
| Weldability | Excellent (MIG, TIG), but welding loses T6 strength | Not arc weldable | Very good |
| Corrosion resistance | Excellent | Vulnerable to stress-corrosion cracking | Excellent in seawater |
Typical figures from Wikipedia (6061-T6, 7075-T651) and Austral Wright Metals (5083, H116/H321 minimum); ratings from BlueScope Distribution, The Fabricator, Wikipedia and Austral Wright.
Practical points to consider when you design a part in Aluminium 7075.
7075 is not arc weldable, so assemblies are normally bolted or riveted.
7075 is vulnerable to stress-corrosion cracking. T7 tempers reduce the risk where that matters.
At about 570 MPa and 2.81 g/cm³, 7075 is used where every gram and every megapascal count.
Highly stressed parts such as aircraft fittings, gears and shafts, valve parts, worm gears, keys, aerospace and defence parts, and bicycle frames.
Compare them all in our material overview or narrow them down with the material selector.
Common questions about Aluminium 7075. Still unsure? Contact us or call +61 3 9764 2749.
Yes. Typical tensile strength is about 570 MPa for 7075-T651, against about 310 MPa for 6061-T6.
Yes. It is anodised like other aluminium alloys.
Not by arc welding: the heat-affected zone is prone to cracking and stress-corrosion cracking, so it is normally fastened.
Please use this information as a guide only. It is a general rapid prototyping reference based on typical results, and many assumptions were made in producing it. It is not a recommendation for any particular application, so please don't use it for product design or engineering decisions. The final choice of process and material is yours; check critical properties with the material manufacturer's data sheets.
Upload your CAD files for a free, obligation-free quote.